| Specific Gravity | g/cm3 | 1.70 |
| Specific Resistance | (??m) | 8.5 |
| Youngs Modulus | (GPa) | n/a |
| Flexural Strength | (MPa) | 15.7 |
| Tensile Hardness | (MPa) | 7.8 |
| Shore Hardness | sHD | 25 |
| C.T.E. | (×10-6/°C) | 3.8 |
| Thermal Conductivity | (W/mk) | 145 |
| Pore Size | ?m | n/a |
| Porosity | % | 20 |
| Max’ Grain Size | ?m | 1 |
| Ave’ Grain Size | ?m | 1 |
| Gas Permeability | cm2/sec | n/a |